Thursday, March 29, 2018

Re: [MW:27578] Re: PWHT required or not for Saddle welded to pipes

Read carefully 132.4 and you will find your answer

2018-03-24 14:42 GMT+02:00 Vairamuthu <vaira.muthu.78@gmail.com>:
Yes. PWHT required as it is directly welded to pressure part.

On Thursday, December 21, 2017 at 9:14:19 AM UTC+3, bapun wrote:
Dear Expert 
                    Kindly help me out to decide whether we have to perform PWHT or not for Pipe to Saddle support fillet welding .Design  Code ASME B 31.1 .The details given below and its a long distance pipe rack job

The saddle material is ASTM A387 GR 11.
The welding type is fillet welding.
HP pipe detail - DN-350,THK-28 mm and Material  ASTM A 335 P11.

--
tHanks & rEgards
Chandra Bhanu Mohapatra

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.



--
Dr. Georgios Dilintas,
Dipl. Ing. In Aeronautic and Space Engineering
Ph.D in Mechanics of Solids - Computational Mechanics
A.I.S, A.N.I, IRCA Lead Auditor
Welding, Stress Analysis, Corrosion, QA/QC, Failure Analysis, Risk Analysis

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...