Re: [MW:27553] Rolling/forming method for Gr.91 Plate

Dear sir,

Thanks for your suggestion..
Still i have some query as below.
1. Our dish dia 26", can we make this diameter in crown & petal type.
2. Is hot rolling/bending is better solution for this if it is then what is the recommended temp & precautions for this.
3. Our plate dish cracks multiple locations, is it recommended to weld repair of these cracks, any chances of delayed cracking, please suggest.

Sir your suggestion will be very helpful for us to out of this problem.

  Thanks & regards,
Brajendra Patel


------ Original message------
From: 'Prakash Hegde' via Materials & Welding
Date: Sat, 24 Mar 2018 10:25
To: materials-welding@googlegroups.com;
Cc:
Subject:Re: [MW:27549] Rolling/forming method for Gr.91 Plate

Hi!
For high alloy steelmaterial edges should be ground and rounded followed by MPT and LPT 
LOADING SHOULD BE GRADUAL and not sudden.during forming
For D.end.it is always better.to go for crown and petal 
Regards
Hegde


On Fri, 23 Mar 2018 at 15:17, Brajendra Singh
<brajendra1020@gmail.com> wrote:
Dear expert's,
Please share the forming/rolling requirements for A387 Gr.91, we have tried cold forming/rolling of shell & dish end but always cracking.
Attaching photographs for refrence.
Thanks in advance

Regards, 
Brajendra Patel
Mob:+917057406907

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.
Think before you print. This e-mail may contain confidential and privileged material for the sole use of the intended recipient. Any review, use, distribution or disclosure by others is strictly prohibited. If you are not the intended recipient (or authorized to receive for the recipient), please contact the sender by reply e-mail and delete all copies of this message. Koso India Pvt Ltd. --- H-33 & 34, MIDC, Ambad, Nashik – 422010, Maharashtra, India ,Tel + 91 253 2408811, Fax + 91 253 2384413
Think before you print. This e-mail may contain confidential and privileged material for the sole use of the intended recipient. Any review, use, distribution or disclosure by others is strictly prohibited. If you are not the intended recipient (or authorized to receive for the recipient), please contact the sender by reply e-mail and delete all copies of this message. Koso India Pvt Ltd. --- H-33 & 34, MIDC, Ambad, Nashik – 422010, Maharashtra, India ,Tel + 91 253 2408811, Fax + 91 253 2384413

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...