Hi

 

Both Structural steel materials falls under group 1 as per ISO /TR 15608 (YS <360  N/mm 2) and its qualified within its group number as per EN ISO 15614-1

 

Screen shots attached for reference








On Fri, Mar 23, 2018 at 4:32 AM, 'Maghroud Moussa' via Materials & Welding <materials-welding@googlegroups.com> wrote:

Dear experts

 

Please can you help to tell me if a PQR made with S275JR ( Process is SMAW 111, E 7018) can supporte welding of S355JR according to EN normes.

 

Best regard

 

Provenance : Courrier pour Windows 10

 

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...