Hi!
For high alloy steelmaterial edges should be ground and rounded followed by MPT and LPT 
LOADING SHOULD BE GRADUAL and not sudden.during forming
For D.end.it is always better.to go for crown and petal 
Regards
Hegde


On Fri, 23 Mar 2018 at 15:17, Brajendra Singh
<brajendra1020@gmail.com> wrote:
Dear expert's,
Please share the forming/rolling requirements for A387 Gr.91, we have tried cold forming/rolling of shell & dish end but always cracking.
Attaching photographs for refrence.
Thanks in advance

Regards, 
Brajendra Patel
Mob:+917057406907

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...