Re: [MW:27547] Welding S355 JR

Materiaal S275 is Group 1 material and for EN ISO 15614-1 base material is an essential parameter. In this case both materials are Group 1 materials but specification also mentions that a material qualified in this Group only qualifies for materials in the same group with equal or lower yield strength. Because of that S275 is not acceptable for covering a WPS for S355.

Verstuurd vanaf mijn iPhone

Op 23 mrt. 2018 om 00:02 heeft 'Maghroud Moussa' via Materials & Welding <materials-welding@googlegroups.com> het volgende geschreven:

Dear experts

 

Please can you help to tell me if a PQR made with S275JR ( Process is SMAW 111, E 7018) can supporte welding of S355JR according to EN normes.

 

Best regard

 

Provenance : Courrier pour Windows 10

 

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...