Why there is RT room size limitation ? Tell him to take RT in night shift by properly cordoning the area .
Regards
Prem Nautiyal
PREM S NAUTIYAL
CELL : 9769316004
From: Makrand Sakpal <makrands9@gmail.com>
Sent: Wed, 21 Mar 2018 19:32:57 GMT+0530
To: Materials & Welding <materials-welding@googlegroups.com>
Subject: [MW:27534] TOFD in lieu of RT
Dears,
Our prospective vendor is offering TOFD for category A & B weld joints instead of RT for a process column due to RT room size limitations. Is it acceptable by ASME SEC VII DIV-1? What will be the joint efficiency in this case to be used in calculations?
--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https:roups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.
--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.
Subscribe to:
Post Comments (Atom)
Re: [MW:35686] HDPE WPS
Refer ASME SEC IX There is separate chapter for Plastic welding . Based on that you have to prepare Sent from my iPhone On 21 Jun 2025, at...
-
Q: What are equivalents for standard Q 235 B (and Q 235 A) for U-channels? ...
-
Definition of buttering from ASME Section IX, QW/QB-492 Definitions: Buttering: the addition of material, by welding, on one or bot...
-
Section I. PRINT READING 3-1. GENERAL a. Drawings . Drawing or sketching is a universal language used to convey all necessary information to...
No comments:
Post a Comment