General information only.
Attached AWS standard may be useful for your reference. ( AWS UGFM ā User's Guide to Filler Metals)
Refer PART E: COPPER AND COPPER-ALLOY for your reference..
Also refer SFA-5.6/SFA-5.6M & SFA-5.7/SFA-5.7M
Also look for your regular consumable supplier recommendation or recommended filler metals selection guide from various consumable manufacturers like M/s. ESAB, ADOR, BOHLER, LINCOLN, KOBELCO & AIR LIQUIDE etc. etc.ā¦
Ensure Weldability / metallurgical compatible.
As u know, You need to have qualified procedure between P.No 1 to P.No (31 -35 ā copper and its alloys) on your requirement basis.
In case buttering / overlay on CS side, qualify the procedure in same wayā¦
Dear Experts,--Have one doubt regarding copper to carbon steel,which filler using this kind of welding .And explain code also
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com .
Visit this group at https://groups.google.com/group/materials-welding .
For more options, visit https://groups.google.com/d/optout .
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.
Comments