Often, when Equitip portable tester fails in accuracy, it is due to wrong application and missing training in how to do.

You need to have stiff support, because the principle is dependent on the "spring return effect".

 

Otherwise: What accuracy do you need (+/- how many HV10?)

 

 

Yours sincerely

Kristian Lund Jepsen

 

M. Sc. Mech. Eng.

Senior Chief Consultant

Piping, Mecanical and Layout

 

D +45 51617324

M +45  23402936

KUJ@ramboll.com

________________________________________

 

Ramboll

Bavnehojvej 5
DK-6700 Esbjerg
Denmark

www.ramboll.com/energy

 

DK REG. NO. 35128417

 

 

From: materials-welding@googlegroups.com [mailto:materials-welding@googlegroups.com] On Behalf Of Kamesh G
Sent: 17. marts 2018 18:51
To: materials-welding@googlegroups.com
Subject: [MW:27523] Portable Hardness Tester

 

Dear Expert,

Can suggest me best portable hardness tester, already tried Equotip & Hartip but failed in accuracy.
pls. give model # and make


--

Thanks,

Regards

G.K

 

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...