Sunday, March 25, 2018

[MW:27564] AWS D1.1- Measuring Preheat and Interpass Temperature location



Dear Experts

Pls refer appl codes/standards and advise correct measuring location for Preheat and Inter-pass Temperature

Question






How far groove joint, preheat and inter-pass temperature shall be measured?

My understanding:-





1-Preheat Temperature shall be measured minimum 3"(75mm) from groove joint
2-Interpass Temperature shall be measures maximum 10mm from groove joint

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...