[MW:27542] Rolling/forming method for Gr.91 Plate

Dear expert's,
Please share the forming/rolling requirements for A387 Gr.91, we have tried cold forming/rolling of shell & dish end but always cracking.
Attaching photographs for refrence.
Thanks in advance

Regards, 
Brajendra Patel