[MW:27513] RE: 27512] popping and cracking

What's the substrate/ base metal on which the stellite is applied. Stellite deposition would require careful welding supervision. Cracking  could be common due to very high hardness involved. Please refer the attached literature for guidance/information.

 

Thanks.

P.Goswami.

 

 

 

From: materials-welding@googlegroups.com [mailto:materials-welding@googlegroups.com] On Behalf Of Jaidev
Sent: March 13, 2018 2:41 PM
To: Materials & Welding <materials-welding@googlegroups.com>
Subject: [MW:27512] popping and cracking

 

One of welder says the stellite 190 rods (Co- Cr-W) are popping and cracking. what does that mean. Any one experienced such issues.

 

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...