Re: [MW:27117] Automated phased array UT on seamless pipe

it depends on your product standard?

On 5 December 2017 at 09:13, Vivek <vivianlogo@gmail.com> wrote:
Dear experts,

Component-8"seamless pipe,sch 160,super duplex.
Application- oil & gas.

Could you please inform codes/standard needed to refer for performing automated phased array UT?

Will ISO10893-12 &API5LC a good combination?

Regards,
Viv

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

No comments:

Re: [MW:35354] Cast-iron welding

1. Preheat joint area(other area, cover with mineral wool). 2. ENiCi or ENiFe-CI. 3. stringer bead. 4. peening is to be done on weldmetal im...