Re: [MW:27113] WPS/PQR qualification

Only if impact test is not required for p1 to p4 joint.



On Mon, 4 Dec 2017 at 6:10 PM, Anil Yarrolu
<anil.yarrolu@gmail.com> wrote:
Dear Experts,
If my PQR is qualified for P4 G1 to P4 G1 with impact tested at -18 Deg C
Also PHWT done at 705-735 Deg C

Can I use same PQR for the welding of P4 G1 ( A335 Gr.11) to P1 G2 ( A516 Gr.70) with PWHT at 675 +/- 10 Deg ?

Regards
Anil YARROLU

On Dec 4, 2017 3:12 PM, "foued oudina" <oudinafou21@gmail.com> wrote:

Dear Colleagues ;

 

 

Could you  please help me, we have welders qualified in SS they can weld DSS.

 

Thanks

 

 

 

 

cid:image001.jpg@01D1D9DB.D92C4F40

OUDINA FOUAD | QC Welding OFF PLOT

Técnicas Reunidas Group

TouatGaz Project – EPCC Processing & Production Facilities

Field Engineering Group                   

Oued Zine, Adrar, Algeria

*  oudina.f@tecnicasreunidas.es

( Ext. 3912

 

 

--
https://materials-welding. blogspot.com/
https://www.linkedin.com/ groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@ googlegroups.com.
Visit this group at https://groups.google.com/ group/materials-welding.
For more options, visit https://groups.google.com/d/ optout.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

No comments:

Re: [MW:35354] Cast-iron welding

1. Preheat joint area(other area, cover with mineral wool). 2. ENiCi or ENiFe-CI. 3. stringer bead. 4. peening is to be done on weldmetal im...