Monday, December 4, 2017

Re: [MW:27103] Qualifications of welders

P no. is different, need to qualify another WPS for that particular material. 




Thanks & Regards,

ASLAB A KHAN
QC INSPECTOR (PIPING & WELDING)


CONTACT NO.  +965 69335803

On Mon, Dec 4, 2017 at 1:27 PM, Pradeep kumar hormis <pkhormis@gmail.com> wrote:
"P" numbers and "F" numbers will be different, So However Essential variables changed. there is no way to follow same WPS's.

Thanks & Regards

PRADEEPKUMAR HORMIS

Mob: +966-58 16 20 710



 
 


 

On Mon, Dec 4, 2017 at 1:21 PM, 'ms viswanathan' via Materials & Welding <materials-welding@googlegroups.com> wrote:
No, because DSS - P number is 10H and A.No-7 and .S.S-   P number is -8 and A.No 8 , essential variables.
 
Regards, M.S.Viswanathan


On Monday, December 4, 2017 12:42 PM, foued oudina <oudinafou21@gmail.com> wrote:


Dear Colleagues ;
 
 
Could you  please help me, we have welders qualified in SS they can weld DSS.
 
Thanks
 
 
 
 
cid:image001.jpg@01D1D9DB.D92C4F40
OUDINA FOUAD | QC Welding OFF PLOT
Técnicas Reunidas Group
TouatGaz Project – EPCC Processing & Production Facilities
Field Engineering Group                   
Oued Zine, Adrar, Algeria
( Ext. 3912
 
 
--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.


--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

No comments:

Re: [MW:35354] Cast-iron welding

1. Preheat joint area(other area, cover with mineral wool). 2. ENiCi or ENiFe-CI. 3. stringer bead. 4. peening is to be done on weldmetal im...