Monday, December 4, 2017

Re: [MW:27101] Qualifications of welders

as per QW423, he can weld with other essentials are in line with requirements

Virus-free. www.avast.com

THANKS & BEST REGARDS,
KG.PANDITHAN, BE, IWE,  AWS-CWI, CSWIP 3.1,
CONSULTANT-WELDING & QUALITY
Mobile no: +919940739349

On Mon, Dec 4, 2017 at 3:46 PM, Hani Al Masry <hanyonalfy@gmail.com> wrote:
Need a lot of details to judge such case 
And the most important what is the SS They can weld (WPS/PQR) and what is the DSS you need to weld (MTC) most of other WPS Parameters is minor 

Regards,
H.A 

On Mon, Dec 4, 2017 at 12:46 PM, foued oudina <oudinafou21@gmail.com> wrote:

Dear Colleagues ;

 

 

Could you  please help me, we have welders qualified in SS they can weld DSS.

 

Thanks

 

 

 

 

cid:image001.jpg@01D1D9DB.D92C4F40

OUDINA FOUAD | QC Welding OFF PLOT

Técnicas Reunidas Group

TouatGaz Project – EPCC Processing & Production Facilities

Field Engineering Group                   

Oued Zine, Adrar, Algeria

*  oudina.f@tecnicasreunidas.es

( Ext. 3912

 

 

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

No comments:

Re: [MW:35354] Cast-iron welding

1. Preheat joint area(other area, cover with mineral wool). 2. ENiCi or ENiFe-CI. 3. stringer bead. 4. peening is to be done on weldmetal im...