There are 2 things which need to be considered.

1. Base Material Impact requirement.

As specified in API 5L which need to be part of MTC and decided based on OD.

2. Welding Procedure Impact test.

It depends on the Design Code and the corresponding fabrication code.

Thanks & Regards

J.Gerald Jayakumar

0091-9344954677



On Sunday, December 3, 2017, 6:22:31 AM GMT+4, Mukul Samad <mukul.hossen.me@gmail.com> wrote:


I just want to know that , when impact test is required ?


On Sunday, August 7, 2016 at 8:40:33 AM UTC+6, perumal govindan wrote:
Dear Experts,

We have the piping material spec. of API 5L Gr. B/ X52/X56 PSL piping materials, MDMT is -3 (North Kuwait) Degree centigrade and thickness ranging from 5 mm to 31 mm.

Please advice whether the impact testing is required to carried during PQT.



With Kind Regards

P Govindan


--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

No comments:

[MW:35633] IP Joint

Hello experts, I would like to know what is IP joints in piping(31.3)?  Regards Saurabh -- https://materials-welding.blogspot.com/...