[MW:27091] Re: Impact Testing requirement for welding procedure qualification

I just want to know that , when impact test is required ?


On Sunday, August 7, 2016 at 8:40:33 AM UTC+6, perumal govindan wrote:
Dear Experts,

We have the piping material spec. of API 5L Gr. B/ X52/X56 PSL piping materials, MDMT is -3 (North Kuwait) Degree centigrade and thickness ranging from 5 mm to 31 mm.

Please advice whether the impact testing is required to carried during PQT.



With Kind Regards

P Govindan


--
https://materials-welding.blogspot.com/
https://www.linkedin.com/groups/122787
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
For more options, visit https://groups.google.com/d/optout.

No comments:

Re: [MW:35354] Cast-iron welding

1. Preheat joint area(other area, cover with mineral wool). 2. ENiCi or ENiFe-CI. 3. stringer bead. 4. peening is to be done on weldmetal im...