Re: [MW:26378] Need clarification about API 1104

Kindly help me

We need to qualify a new PQR for 66" 18mm thick in service welding. Please note that our sleeve thickness is 20mm. the longitudinal welding with backing strip and direct run pipe welding is fillet weld. Kindly help me the PQR pipe thickness requirements since the thickness range qualification is silent in API 1104 for in service welding.

Ashique.K.V

On Tuesday, March 1, 2011 at 2:54:05 PM UTC+3, Fitria Rahman wrote:
Yes, B.2.2.1.3 does not specify that wall thickness is an essential variable. But first of all, wall thickness of the pipe should be considered against thermal severity of the piping during in service. accepted minimum thk is 4.8mm (0.118").

Let this helps

Rgds,

2011/3/1 James, GeraldJayakumar <GeraldJaya...@fwuk.fwc.com>

Sleeve longitudinal welding  & Branch welding will be covered by API 1104 clause 6.2.2.e

 

In Sleeve to Pipe Fillet weld, the wall thickness is not an essential variable according to API 1104 clause B2.2.1.3 Appendix B

 

J.Gerald

 

From: material...@googlegroups.com [mailto:material...@googlegroups.com] On Behalf Of joshi jaydeep
Sent: Tuesday, March 01, 2011 3:30 PM
To: material...@googlegroups.com
Subject: [MW:10069] Need clarification about API 1104

 

Dear all,
 


API 1104 Clause No. 6.2.2 (e) mentions about the 'Pipe wall thickness grouping' as an essential variable.
 
If we have a requirement of welding a sleeve on Pipe (as in-service weld), do we need to consider the Sleeve thickness as an essential variable?
 
I believe API 1104 code is silent about the Sleeve thickness.
 
Please guide.
 
 
 Thanks and Regards,
 

Jaydeep Joshi |Welding Engineer, TDW India Limited

Plot No 16 | Phase –III | Alindra – Savli G.I.D.C | Taluka : Savli | Vadodara – 391 775

Board : +91-2667- 619900 | Fax : +91- 2667- 619501| Extension : 7845

E-Mail : jaydeep.joshi@tdwilliamson.com  | www.tdwilliamson.com

Cell: +91 9978959626

P    Before printing, Think about ENVIRONMENTAL responsibility

--
To post to this group, send email to material...@googlegroups.com
To unsubscribe from this group, send email to materials-weld...@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.


Confidentiality Notice

This communication and the information it contains:-
(a) Is intended for the person(s) or organisation(s) named above and for no other person(s) or organisation(s).
(b) May be confidential, legally privileged and protected in law. Unauthorised use, copying or disclosure of any of it may be unlawful. If you have received this communication in error, please contact us immediately by email at Postm...@fwuk.fwc.com.

--
To post to this group, send email to material...@googlegroups.com
To unsubscribe from this group, send email to materials-weld...@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.

--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/4abbbbb4-3cf2-4b39-a739-5b3837f7a914%40googlegroups.com.
For more options, visit https://groups.google.com/d/optout.

Comments

Popular posts from this blog

Materails FAQs

Q: What are equivalents for standard Q 235 B (and Q 235 A) for U-channels? (asked by: boris.vielhaber@vait.com) A: DIN Nr. = 2393 T.2, 2394 T.2, EN 10025 W. Nr. DIN 17007 = 1.0038 Design DIN 17006 = RSt 37-2, S235JRG2 (Fe 360 B) Q: What is St DIN 2391 BK material? (asked by: dmcandrews@automaticstamp.com) A: Precision steel tubes, cold-finished/hard. Q: What is C.D.W. Boiler Tube? (asked by: montydude123@yahoo.com) A: Cold Drawn Welded Boiler Tube. Q: WHAT IS W.Nr. 1.4301? PLS TELL US IN EASY LANGUAGUE (asked...

[MW:36169] Cold Bending Qualification

Dear Experts,  Can anyone share the inspection requirements or a qualification procedure for cold bending? Our client spec states only the requirements for induction bending and would like to know your opinion on the cold bend inspection requirements. The code of construction is B31.3, Max. 5D bends, A106 SS 316L.  Thanks in Advance. -- https://materials-welding.blogspot.com/ https://www.linkedin.com/groups/122787 --- You received this message because you are subscribed to the Google Groups "Materials & Welding" group. To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com . To view this discussion visit https://groups.google.com/d/msgid/materials-welding/1be61cc3-e9c9-4a5f-834d-e8485e248432n%40googlegroups.com .

Heat tint (temper) colours on stainless steel surfaces heated in air // Heat tint

Introduction The colour formed when stainless steel is heated, either in a furnace application or in the heat affected zone of welds, is dependent on several factors that are related to the oxidation resistance of the steel. The heat tint or temper colour formed is caused by the progressive thickening of the surface oxide layer and so, as temperature is increased, the colours change.   Oxidation resistance of stainless steels However, there are several factors that affect the degree of colour change and so there is no a single table of colour and temperature that represents all cases. The colours formed can only be used as an indication of the temperature to which the steel has been heated. Factors affecting the heat tint colours formed Steel composition The chromium content is the most important single factor affecting oxidation resistance. The higher the chromium, the more heat resistant the steel and so the development of the heat tint colou...