Skip to main content

RE: [MW:26414] PAUT (Phased Array Ultrasonic Testing)

Hi Ganesan,

 

ASME code case 2235-9 allows this technique for DIV-1 construction, in lieu of RT. The following links will help you to understand the complications involved.

 

As stated below by Prakash Hegde establishing the integrity, reliability  of this technique in additional to operators' qualification and experience is important. So as convincing the AI s.

 

As regarding this technique, please go through ASME Sec V. Requirements of technique and other requirements are clarified in details.

 

Thanks.

 

 

P.Goswami.P.Eng, IWE.

Welding & Metallurgical Specialist

Linkedin: https://www.linkedin.com/in/pradip-goswami-2999855/

Email:pgoswami@quickclic.net,pradip.goswami@gmail.com

 

1.       http://endalloy.net/CODECASE2235EN.pdf

2.       http://www.ndt.net/article/jrc-nde2012/papers/84.pdf

3.       http://www.olympus-ims.com/en/applications/ultrasonic-phased-array-in-lieu-of-radiography/

 

From: 'Prakash Hegde' via Materials & Welding [mailto:materials-welding@googlegroups.com]
Sent: April 14, 2017 3:57 AM
To: materials-welding@googlegroups.com
Subject: Re: [MW:26412] PAUT (Phased Array Ultrasonic Testing)

 

Hi Firend

P/Array is reliable method can be used in liu of RT and very fast and no hazard

However you should have instrument and qualified person to carry and interprete the process

 

There are NDE/NDT vendors who take up the NDE by  P/Array  However you require to qualify the mock up prior to NDE test  depends upon thk,Metallurgy etc

Regards

Hegde

 

On Friday, 14 April 2017 11:04 AM, 'Ganesan' via Materials & Welding <materials-welding@googlegroups.com> wrote:

 

Dear Experts,

 

Can you please guide me regarding PAUT (Phased Array Ultrasonic Testing) instead of RT. Our contractor has recommended PAUT due to RT process is slow and it will be affected the project schedule. So, they are pressuring us to do PAUT instead of RT.  

 

Is it good NDT technique & which standard shall i follow for the acceptance criteria. 

 

Please share the testing method and acceptance criteria, if anyone have.

 

I'm waiting for your valuable advise in this regard.     

 

Thanks & Regards, K.GANESAN Quality Control ISGEC / ISGEC John Thompson, A-4 Sector-24 Noida-201301 (UP) Tel. +91-120-2411175 Direct Tel. +91-120-2411175 Mobile : +91-9952166894

--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/1547052087.1269331.1492067703665%40mail.yahoo.com.
For more options, visit https://groups.google.com/d/optout.

 

--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/1696905942.234574.1492156622011%40mail.yahoo.com.
For more options, visit https://groups.google.com/d/optout.




AVG logo

This email has been checked for viruses by AVG antivirus software.
www.avg.com


Comments

Popular posts from this blog

Materails FAQs

Q: What are equivalents for standard Q 235 B (and Q 235 A) for U-channels? (asked by: boris.vielhaber@vait.com) A: DIN Nr. = 2393 T.2, 2394 T.2, EN 10025 W. Nr. DIN 17007 = 1.0038 Design DIN 17006 = RSt 37-2, S235JRG2 (Fe 360 B) Q: What is St DIN 2391 BK material? (asked by: dmcandrews@automaticstamp.com) A: Precision steel tubes, cold-finished/hard. Q: What is C.D.W. Boiler Tube? (asked by: montydude123@yahoo.com) A: Cold Drawn Welded Boiler Tube. Q: WHAT IS W.Nr. 1.4301? PLS TELL US IN EASY LANGUAGUE (asked...

[MW:36169] Cold Bending Qualification

Dear Experts,  Can anyone share the inspection requirements or a qualification procedure for cold bending? Our client spec states only the requirements for induction bending and would like to know your opinion on the cold bend inspection requirements. The code of construction is B31.3, Max. 5D bends, A106 SS 316L.  Thanks in Advance. -- https://materials-welding.blogspot.com/ https://www.linkedin.com/groups/122787 --- You received this message because you are subscribed to the Google Groups "Materials & Welding" group. To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com . To view this discussion visit https://groups.google.com/d/msgid/materials-welding/1be61cc3-e9c9-4a5f-834d-e8485e248432n%40googlegroups.com .

Heat tint (temper) colours on stainless steel surfaces heated in air // Heat tint

Introduction The colour formed when stainless steel is heated, either in a furnace application or in the heat affected zone of welds, is dependent on several factors that are related to the oxidation resistance of the steel. The heat tint or temper colour formed is caused by the progressive thickening of the surface oxide layer and so, as temperature is increased, the colours change.   Oxidation resistance of stainless steels However, there are several factors that affect the degree of colour change and so there is no a single table of colour and temperature that represents all cases. The colours formed can only be used as an indication of the temperature to which the steel has been heated. Factors affecting the heat tint colours formed Steel composition The chromium content is the most important single factor affecting oxidation resistance. The higher the chromium, the more heat resistant the steel and so the development of the heat tint colou...