Dear Pradip


Thank you for reply, but actually my doubt is still remain, as you can see in Table SA-350 there is no difference between LF1 and LF2 grades in chemical composition range, so I have confused about mechanical properties (as you mentioned tensile and impact properties), meanwhile as I already stated in my 1st email, this difference in impact test is also in two class of LF2, I want to know the reason for these differences despite of similar chemical composition.


Regards,

Himan Nikdin


From: materials-welding@googlegroups.com <materials-welding@googlegroups.com> on behalf of PGoswami <pgoswami@quickclic.net>
Sent: Saturday, April 15, 2017 1:57:31 AM
To: materials-welding@googlegroups.com
Subject: RE: [MW:26414] Difference between A350 LF1 and LF2
 

Hi Himan,

 

Please look at the extract from Table-2 of Specification SA350.

 

Although the compositional requirements are overlapping, 350 LF1 closer to P1Gr1 material(e.g. SA 516/60, plates), while 350LF2 is closer to P1 Gr 2 material(e.g. SA 516/70, plates).

 

It's the compositional differences, lower C and higher Mn which makes major differences in the properties for these grades of forgings.

 

Also if you look at Table-3, you'll note there are differences in the required  impact test values(Full Size specimen) for both materials.

 

Hope this will clarify your doubt.

 

Thank.

 

 

P.Goswami.P.Eng, IWE.

Welding&Metallurgical Specialist

Linkedin: https://www.linkedin.com/in/pradip-goswami-2999855/

Email:pgoswami@quickclic.net,pradip.goswami@gmail.com

 

From: materials-welding@googlegroups.com [mailto:materials-welding@googlegroups.com] On Behalf Of Himan Nikdin
Sent: April 14, 2017 3:44 AM
To: materials-welding@googlegroups.com
Subject: Re: [MW:26410] Differnce between A350 LF1 and LF2

 

Dear George

 

I do not disagree with you, but different grain size is achievable by different chemical composition and/or heat treatment, but I can't find any different chemical composition or heat treatment.

 

Regards,

Himan Nikdin


From: materials-welding@googlegroups.com <materials-welding@googlegroups.com> on behalf of George Dilintas <dilintas@gmail.com>
Sent: Wednesday, April 12, 2017 10:44:39 PM
To: Meghanadh K
Subject: Re: [MW:26403] Differnce between A350 LF1 and LF2

 

Grain Size

 

2017-04-11 16:59 GMT+03:00 Himan Nikdin <himan.nikdin@outlook.com>:

Dear Experts,

Good Day!!

 

I have query regarding SA350 LF1 and LF2, as you can compare the chemical composition of two grades, there are no difference between two grades;

but you can see the major difference between impact test temperature, what is the reason for this major difference as in SA-350 there is no major heat treatment requirements.

also what is the reason for difference between impact test temperature of LF2 Class 1 and class 2?

thanks indeed if you share your valuable ideas.

 

Regards,

Himan Nikdin

--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/DB6PR0902MB1717D3B2FCC67FCBD4651C9C9E000%40DB6PR0902MB1717.eurprd09.prod.outlook.com.
For more options, visit https://groups.google.com/d/optout.



 

--

Dr. Georgios Dilintas,

Dipl. Ing. In Aeronautic and Space Engineering

Ph.D in Mechanics of Solids - Computational Mechanics

A.I.S, A.N.I, IRCA Lead Auditor

Welding, Stress Analysis, Corrosion, QA/QC, Failure Analysis, Risk Analysis

--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAPOi40BLmdZFddAfakdzAjVprEX1VN5rCS%2BsVt%2BdCujfBtJ2%2Bg%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.

--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/DB6PR0902MB17175B80F2B15824D0C7B2F89E050%40DB6PR0902MB1717.eurprd09.prod.outlook.com.
For more options, visit https://groups.google.com/d/optout.




AVG logo

This email has been checked for viruses by AVG antivirus software.
www.avg.com


--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/!%26!AAAAAAAAAAAYAAAAAAAAAB/s9XS594ZCoMHlmX4xaZ3CgAAAEAAAAEbuIG2s7UhIjfHP3IFGcPMBAAAAAA%3D%3D%40quickclic.net.
For more options, visit https://groups.google.com/d/optout.

Comments

Popular posts from this blog

Materails FAQs

Q: What are equivalents for standard Q 235 B (and Q 235 A) for U-channels? (asked by: boris.vielhaber@vait.com) A: DIN Nr. = 2393 T.2, 2394 T.2, EN 10025 W. Nr. DIN 17007 = 1.0038 Design DIN 17006 = RSt 37-2, S235JRG2 (Fe 360 B) Q: What is St DIN 2391 BK material? (asked by: dmcandrews@automaticstamp.com) A: Precision steel tubes, cold-finished/hard. Q: What is C.D.W. Boiler Tube? (asked by: montydude123@yahoo.com) A: Cold Drawn Welded Boiler Tube. Q: WHAT IS W.Nr. 1.4301? PLS TELL US IN EASY LANGUAGUE (asked...

[MW:36169] Cold Bending Qualification

Dear Experts,  Can anyone share the inspection requirements or a qualification procedure for cold bending? Our client spec states only the requirements for induction bending and would like to know your opinion on the cold bend inspection requirements. The code of construction is B31.3, Max. 5D bends, A106 SS 316L.  Thanks in Advance. -- https://materials-welding.blogspot.com/ https://www.linkedin.com/groups/122787 --- You received this message because you are subscribed to the Google Groups "Materials & Welding" group. To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com . To view this discussion visit https://groups.google.com/d/msgid/materials-welding/1be61cc3-e9c9-4a5f-834d-e8485e248432n%40googlegroups.com .

Heat tint (temper) colours on stainless steel surfaces heated in air // Heat tint

Introduction The colour formed when stainless steel is heated, either in a furnace application or in the heat affected zone of welds, is dependent on several factors that are related to the oxidation resistance of the steel. The heat tint or temper colour formed is caused by the progressive thickening of the surface oxide layer and so, as temperature is increased, the colours change.   Oxidation resistance of stainless steels However, there are several factors that affect the degree of colour change and so there is no a single table of colour and temperature that represents all cases. The colours formed can only be used as an indication of the temperature to which the steel has been heated. Factors affecting the heat tint colours formed Steel composition The chromium content is the most important single factor affecting oxidation resistance. The higher the chromium, the more heat resistant the steel and so the development of the heat tint colou...