Re: [MW:25261] Basic rule for selection of consumable for piping

Dear Mustaq,

Since you mentioned B.31.3  for the proper consumable selection , please specify the process.
is it  GTAW+SMAW   combination  or full SMAW?
 

Best Regards,

JIJILAL K.M. 



On 16 August 2016 at 00:45, 'c sridhar' via Materials & Welding <materials-welding@googlegroups.com> wrote:
For CS, minimum min. UTS values of consumable selected  must be just above the 
values of min. base metal. Chemistry is not a criteria as it may differ from base toweld chemistry.

For your 106 Gr. B pipe,it could be,

1. E 6013 for root, filler cap  or 
2. E 6010 for root and E 6013 for F & C. or
4. E 6013 for root and E 7018 for F & C  or
4. E 7016 for root and E 7018 for F & C (used in shipyards) or
5. E 7018 throughout.

1 & 2 are common in plant piping. 

For AS & SS , chemistry of base mental is the criteria and not UTS values.

Trust it is useful to you.
Sridhar.
---------------------------------------------------------------------------------------------------






From: 'anand gupta' via Materials & Welding <materials-welding@googlegroups.com>
To: "materials-welding@googlegroups.com" <materials-welding@googlegroups.com>; Mustaq Ahmad <mustaqnk@gmail.com>; Materials & Welding <materials-welding@googlegroups.com>
Sent: Tuesday, 9 August 2016 9:07 PM
Subject: Re: [MW:25236] Basic rule for selection of consumable for piping

Dear
minimum base matel tensile and chemical composition is required or higher will acceptable. 

A p gupta
baroda


On Tue, 9 Aug, 2016 at 18:38, Mustaq Ahmad
Dear experts

I am working as QC-ENGINEER, as I am preparing wps/pqr 1st time,I need some guidance regarding consumable selection like what are criteria to be considered,
Example for b31.3 and  section IX is the code carbon steel is material A106grB pipe. In this how we select from sectionII part C

Regards
Mustaq

--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/0568c66f-2bc8-4c9a-8794-b82f6a6d137b%40googlegroups.com.
For more options, visit https://groups.google.com/d/optout.
--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/1802857053.10716575.1470757039517.JavaMail.yahoo%40mail.yahoo.com.
For more options, visit https://groups.google.com/d/optout.


--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/1102423112.13169676.1471283143333.JavaMail.yahoo%40mail.yahoo.com.
For more options, visit https://groups.google.com/d/optout.

--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAHmEnHgZw-KmoMg40tBDTrUOZX8_gSSAh0izdH9x%3DmdyN56LJg%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.

Comments

Popular posts from this blog

Materails FAQs

Q: What are equivalents for standard Q 235 B (and Q 235 A) for U-channels? (asked by: boris.vielhaber@vait.com) A: DIN Nr. = 2393 T.2, 2394 T.2, EN 10025 W. Nr. DIN 17007 = 1.0038 Design DIN 17006 = RSt 37-2, S235JRG2 (Fe 360 B) Q: What is St DIN 2391 BK material? (asked by: dmcandrews@automaticstamp.com) A: Precision steel tubes, cold-finished/hard. Q: What is C.D.W. Boiler Tube? (asked by: montydude123@yahoo.com) A: Cold Drawn Welded Boiler Tube. Q: WHAT IS W.Nr. 1.4301? PLS TELL US IN EASY LANGUAGUE (asked...

[MW:36169] Cold Bending Qualification

Dear Experts,  Can anyone share the inspection requirements or a qualification procedure for cold bending? Our client spec states only the requirements for induction bending and would like to know your opinion on the cold bend inspection requirements. The code of construction is B31.3, Max. 5D bends, A106 SS 316L.  Thanks in Advance. -- https://materials-welding.blogspot.com/ https://www.linkedin.com/groups/122787 --- You received this message because you are subscribed to the Google Groups "Materials & Welding" group. To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com . To view this discussion visit https://groups.google.com/d/msgid/materials-welding/1be61cc3-e9c9-4a5f-834d-e8485e248432n%40googlegroups.com .

Heat tint (temper) colours on stainless steel surfaces heated in air // Heat tint

Introduction The colour formed when stainless steel is heated, either in a furnace application or in the heat affected zone of welds, is dependent on several factors that are related to the oxidation resistance of the steel. The heat tint or temper colour formed is caused by the progressive thickening of the surface oxide layer and so, as temperature is increased, the colours change.   Oxidation resistance of stainless steels However, there are several factors that affect the degree of colour change and so there is no a single table of colour and temperature that represents all cases. The colours formed can only be used as an indication of the temperature to which the steel has been heated. Factors affecting the heat tint colours formed Steel composition The chromium content is the most important single factor affecting oxidation resistance. The higher the chromium, the more heat resistant the steel and so the development of the heat tint colou...