Skip to main content

[MW:25304] Re: Free NDT online course

Le mardi 3 juin 2008 09:12:48 UTC+1, Sankepalli R.S.Reddy a écrit :
> Good day all,
>
>  
>
> The web link below is providing free online NDT courses which cover: MT, PT, UT, RTFI.
>
>
> It's a very useful and full of information NDT site which will add more information to what you got and will
>
>
> help you in your NDT certifications exam.
>
>  
>
> No registration, no fees required and you can get a direct evaluation score by utilizing the course quizzes.  
>
>
> Please see attached, an example of a course material regarding Radiograph Interpretation - Welds
>
>
>  
>
> Shortcut to: http://www.ndt-ed.org/EducationResources/CommunityCollege/communitycollege.htm
>
>
>  
>
>  
>
> SRSReddy
>
> Aramco
>
>  
Huge discount! Check out 3 #Udemy Courses for free! Please leave a review when you finish takinng the lectures. This is the last round of free coupons on my courses ever! *********************************************************************************** 100% Off: Fundamentals of #Ultrasonic_Testing * Learn the basic theoretical knowledges and practical skills of UT required for a Level I (1) technician * Complete calibration of ultrasonic flaw detection equipment for various types of transducers, Discontinuity Detection, Locating the flaw and Size Estimation Techniques. * Carry out tests according to an established procedure under the supervision of a level II (2) or level III (3) personnel. https://www.udemy.com/ultrasonic-testing/?couponCode=LAST-CHANCE *********************************************************************************** 100% off ===> #Twitter #Marketing Automation Do you want to grow your twitter audience by getting huge amounts of followers every day for free? Do you want to start promoting your business via twitter DMs and tweets? Do you want your twitter account to be automated so you can get more leads while you sleep? If yes, I have a free online course that will help you achieve all that! Just remember me when you hit the big days by leaving a review and feel free to pass the savings to any worthy friends as the regular price of this course is $20. Don't waste more time! Just use the link bellow or reedem " OnlyYou " as a coupon code to get your 100% discount! www.udemy.com/twitter-growth-hacking/?couponCode=OnlyYou *********************************************************************************** 100% off ===> Fundamentals of #Project_Management Do you want to: * Ensure that your projects are set-up for success from the start by building a solid foundation of project management knowledge, techniques and tools? * Develop an integrated project plan including realistic scope, schedules, budgets, and risks and turn that plan into successful action? * Gather and document requirements? * Track and report on project progress in the most effective way? * Gain the respect of your project team and build credibility with top management? If Yes, The solution is here: The comprehensive guide for newbies to successfully learn project management and easily get the #PMP certification is available for free on udemy Please remember me when you hit the big days by leaving a review and share the savings with your worthy friends! Limited coupons for limited time Hurry up! http://www.freeudemycourses.info/2016/07/udemy-100-off-projectmanagement.html

--
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/f6b04c8c-468e-487b-82a1-4ed85ed88c53%40googlegroups.com.
For more options, visit https://groups.google.com/d/optout.

Comments

Popular posts from this blog

Materails FAQs

Q: What are equivalents for standard Q 235 B (and Q 235 A) for U-channels? (asked by: boris.vielhaber@vait.com) A: DIN Nr. = 2393 T.2, 2394 T.2, EN 10025 W. Nr. DIN 17007 = 1.0038 Design DIN 17006 = RSt 37-2, S235JRG2 (Fe 360 B) Q: What is St DIN 2391 BK material? (asked by: dmcandrews@automaticstamp.com) A: Precision steel tubes, cold-finished/hard. Q: What is C.D.W. Boiler Tube? (asked by: montydude123@yahoo.com) A: Cold Drawn Welded Boiler Tube. Q: WHAT IS W.Nr. 1.4301? PLS TELL US IN EASY LANGUAGUE (asked...

[MW:36169] Cold Bending Qualification

Dear Experts,  Can anyone share the inspection requirements or a qualification procedure for cold bending? Our client spec states only the requirements for induction bending and would like to know your opinion on the cold bend inspection requirements. The code of construction is B31.3, Max. 5D bends, A106 SS 316L.  Thanks in Advance. -- https://materials-welding.blogspot.com/ https://www.linkedin.com/groups/122787 --- You received this message because you are subscribed to the Google Groups "Materials & Welding" group. To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com . To view this discussion visit https://groups.google.com/d/msgid/materials-welding/1be61cc3-e9c9-4a5f-834d-e8485e248432n%40googlegroups.com .

Heat tint (temper) colours on stainless steel surfaces heated in air // Heat tint

Introduction The colour formed when stainless steel is heated, either in a furnace application or in the heat affected zone of welds, is dependent on several factors that are related to the oxidation resistance of the steel. The heat tint or temper colour formed is caused by the progressive thickening of the surface oxide layer and so, as temperature is increased, the colours change.   Oxidation resistance of stainless steels However, there are several factors that affect the degree of colour change and so there is no a single table of colour and temperature that represents all cases. The colours formed can only be used as an indication of the temperature to which the steel has been heated. Factors affecting the heat tint colours formed Steel composition The chromium content is the most important single factor affecting oxidation resistance. The higher the chromium, the more heat resistant the steel and so the development of the heat tint colou...