Thursday, February 4, 2016

[MW:24229] Re: Filler wire for SA312 TP316H using GTAW process

Can we use ERNiCrMo3 ??


On Saturday, January 16, 2016 at 4:51:34 AM UTC+3, sachin kumar wrote:

Dear Expert,
Can we use ER316 for welding of SA312 TP316H piping by GTAW process.
Regards,
Sachin

--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/ba45e45a-3be7-43e2-be7d-fd3394a074c3%40googlegroups.com.
For more options, visit https://groups.google.com/d/optout.

No comments:

Re: [MW:35289] Welding consumable for S355J2WP material

S355 J2 WP  is a weathering structural steel  It has better atmospheric corrosion resistance. Use E 8018 - W1/W2  Electrodes This is regular...