so it means that UT for these type of material is limited/prohibited, but this is not raised in American standards.
Date: Wed, 3 Feb 2016 16:26:08 +0530
Subject: Re: [MW:24222] UT limitation
From: kadirgodil@gmail.com
To: materials-welding@googlegroups.com
--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAKaLp%2BVF71Ccs-5WreEQ6JgqF_S8%2B%3DjJvVpdTLp04thhhZ0G1A%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.
Date: Wed, 3 Feb 2016 16:26:08 +0530
Subject: Re: [MW:24222] UT limitation
From: kadirgodil@gmail.com
To: materials-welding@googlegroups.com
Austenitic structure has large grains boundaries. this GB hinders the movement of sound waves. this causes Attenuation of sound waves thts why...
On Wed, Feb 3, 2016 at 1:38 PM, Himan Nikdin <himan.nikdin@outlook.com> wrote:
Dear Experts
Good day!!!!
Refer to EN ISO 15614-1 "Ultrasonic testing shall not be used for t < 8 mm and not for material groups 8, 10, 41 to 48"
Where group 8 is Austenitic Stainless Steel, group 10 is duplex stainless steels and groups 41 to 48 are nickel alloys, As the Austenitic structure is common between the mentioned material groups, it seems that the limitation is related to this structure; why???
Meanwhile I have not seen this limitation in US standards.
Regards,
Himan Nikdin
--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/BLU180-W297A90866068443CB0203E9ED00%40phx.gbl.
For more options, visit https://groups.google.com/d/optout.
--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
Visit this group at https://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAKaLp%2BVF71Ccs-5WreEQ6JgqF_S8%2B%3DjJvVpdTLp04thhhZ0G1A%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.
No comments:
Post a Comment