Friday, October 2, 2015

[MW:23645] IMPACT TEST REQUIRMENT AS PER ASME 31.3

Dear Experts,

In our project we qualified The PQR as per sec IX, Material X-65 (GROUP-2),consumable: E8010-P1& E8018GH4R,thk 11.91
.PROCESS: SMAW. PROJECT: PIPELINE. service GAS line.
client requirement is the impact testing shall be conduct at the design metal temperature or 0deg c which ever is lower.
So we take account from our PMS MDMT is -18degc, each consumable we done the impact test including sub size size specimen temperature penalty also calculated.

1. E-8010-P1 specimen size is 3mm penalty temperature is 22.2deg as per31.3 table 323.3.4 (design temperature + penalty)= -41deg c.
2. E-8018GH4R specimen size is 8mm  no penalty impact temperature is same as MDMT -18deg c.

Accordingly above mentioned list we followed and conducted impact test  also passed , now the client questing why you done the high value impact test conducted.

Please advice is there any wrong calculation. if wrong please correct me.

 
Inline image
Inline image
Inline image

 
Regards,
Srinivasan.M

No comments:

Re: [MW:35289] Welding consumable for S355J2WP material

S355 J2 WP  is a weathering structural steel  It has better atmospheric corrosion resistance. Use E 8018 - W1/W2  Electrodes This is regular...