Friday, October 2, 2015

RE: [MW:23641] FW: NEED ADVISE CORROSION IN INHIBITOR TANK REGD

Try coating with thermal sprayed aluminum.

 

Feng Lu

 

From: materials-welding@googlegroups.com [mailto:materials-welding@googlegroups.com] On Behalf Of pgoswami
Sent: Tuesday, September 29, 2015 9:28 PM
To: materials-welding@googlegroups.com
Cc: neilashkumar@yahoo.com
Subject: [MW:23613] FW: NEED ADVISE CORROSION IN INHIBITOR TANK REGD

 

Hi Neileshkumar,

What're the surrounding operating or environmental conditions around the tank. Are there any acid fumes involved. Looks like this tank was not insulated at all??? Is that true.

Appreciate more information on the operating conditions.

 

Thanks


 
Pradip Goswami, P.Eng,IWE
Welding & Metallurgical Engineering Specialist
Hamilton, Ontario, Canada
pgoswami@quickclic.net
pradip.goswami@gmail.com
ca.linkedin.com/pub/pradip-goswami/5/985/299

-----Original Message-----
From: Neilash Kumar [mailto:neilashkumar@yahoo.com]
Sent: Tuesday, September 29, 2015 2:45 AM
To: Pgosami Sir; Pgosami sir
Subject: NEED ADVISE CORROSION IN INHIBITOR TANK REGD

Dear Sir,

Good Morning, please find the attached tank drawing fabricated by us for our client & it is corroded fully , Can you please clarify,

1. Why the tank are corroded So fast?
2. Can you please advise us the method to stop /reduce the rate of corrosion by applying a top coat &  what type of coating to be applied?

please advise me . Material is 316L tank.

Regards
P.Neilashkumar

--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
Visit this group at http://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/0B2230C4544741E7BC1C50621C281EEA%40homepg.
For more options, visit https://groups.google.com/d/optout.

No comments:

Re: [MW:35289] Welding consumable for S355J2WP material

S355 J2 WP  is a weathering structural steel  It has better atmospheric corrosion resistance. Use E 8018 - W1/W2  Electrodes This is regular...