[MW:23644] ASME B31.3_2014- 341.3.3

Dear Sirs

341.3.3 Defective Components and Workmanship
341.3.4 Progressive Sampling for Examination.
When required spot or random examination reveals a defect, then
(a) two additional samples of the same kind (if welded or bonded joints, by the same welder, bonder, or operator) from the original designated lot shall be
given the same type of examination
What does it exactly means by stating " two additional samples of the same kind"

My understanding is
1- Can be 2 additional joints-100% NDT( same type of examination )    OR
2- 2 additional  films on another joint welded by same welder/operatot.

Pls advise
Thanks

--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
Visit this group at http://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/730818f2-9c6f-4b4f-a181-8ea866426c1e%40googlegroups.com.
For more options, visit https://groups.google.com/d/optout.

No comments:

Re: [MW:35289] Welding consumable for S355J2WP material

S355 J2 WP  is a weathering structural steel  It has better atmospheric corrosion resistance. Use E 8018 - W1/W2  Electrodes This is regular...