[MW:23643] ASME B31.3-2014- 331.2.6 Localized Heat Treatment after weld defect repair


Dear Sirs

Pls advise if it is acceptable to ASME B31.3 Code.

Base Material Group - P1 x 10" dia x Sch 160.
Weld Process- GTAW and FCAW.

Carried out RT after PWHT.
Found 30mm defect at 9 o'clock position . Repaired.

Can i perform localized reheat treatment overlapping defect repaired location at least 100mm on both ends?


Thanks



--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
Visit this group at http://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/55ac0a8f-a5f2-4e24-9822-4d9b0f90a613%40googlegroups.com.
For more options, visit https://groups.google.com/d/optout.

No comments:

Re: [MW:35289] Welding consumable for S355J2WP material

S355 J2 WP  is a weathering structural steel  It has better atmospheric corrosion resistance. Use E 8018 - W1/W2  Electrodes This is regular...