I agree

Sent from my BlackBerry 10 smartphone.
From: Shadab Ansari
Sent: Δευτέρα, 31 Αυγούστου 2015 - 20:58
To: materials-welding@googlegroups.com
Reply To: materials-welding@googlegroups.com
Subject: Re: [MW:23374] PWHT requirement for vessel

No. Since its a non-pressure part.

On Aug 29, 2015 5:04 PM, "Prasad" <prsgne@gmail.com> wrote:
Construction Code ASME Sec. VIII Div. 1 Edn. 2013
Non pressure Part skirt support
of vertical vessel not welded directly to vessel.
MOC IS 2062 P no.1 Group  1
Thk. 40 mm
No special service requirement.

For this case whether PWHT is mandatory?

Regards,
Prasad G.

--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
Visit this group at http://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/d725eb3d-aca0-435c-ba4c-feadeba7f303%40googlegroups.com.
For more options, visit https://groups.google.com/d/optout.

--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
Visit this group at http://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CA%2BEkGZc7hH9jjr5xvft3Oyfx3XYxTQ1Pc-7xwuD_KFs-Sj3DKQ%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.

This message contains confidential information. To know more, please click on the following link: http://disclaimer.bureauveritas.com

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...