We have a brosure by Polysoude,the manufacturer. But the limitations are wide. Be cos the manufacturer parameters are commonly used for all material.
But everybody know about the parameters are related with position,size,thickness,metals, layers.
Anybody doing with the polysoude orbital machine, share the news about there.
--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
Visit this group at http://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/b4540d14-3992-4758-97c3-8ac87a0cde21%40googlegroups.com.
For more options, visit https://groups.google.com/d/optout.
Subscribe to:
Post Comments (Atom)
[MW:35614] Re: SS FILLER
dear , pl check A number and Gas composition use for ss cant be sutibale same % for duplex., u need to qualified with aditional testing of f...
-
Q: What are equivalents for standard Q 235 B (and Q 235 A) for U-channels? ...
-
Definition of buttering from ASME Section IX, QW/QB-492 Definitions: Buttering: the addition of material, by welding, on one or bot...
-
Section I. PRINT READING 3-1. GENERAL a. Drawings . Drawing or sketching is a universal language used to convey all necessary information to...