Previously the selected material for tanks construction was SA-516 Gr. 70 but to unavailability of selected material in the market, a comparison was made b/w chemical composition and mechanical properties of easily available material i.e. S355J2 and selected for construction instead of SA-516 Gr. 70. Now the question is that we have PQR for SA-516 Gr. 70 and the referenced WPS is listed with new material i.e. S355J2. can we use use these WPS and PQR?