[MW:23239] Dilution calculation for inconel to ds groove weld with GTAW

Dear all,
I have Inconel 600 to SS 304 joint.
Process is GTAW.
Filler wire ERNiCr-3
joint design is single V.
Dilution consider 25%.

How to calculate final weld composition?

Thank you.

Hrushikesh H Sangamnerkar

--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
Visit this group at http://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAMpWL2qHVuFOVJAXn2G-VrJsLOLsjjcJtVV1VQt2HYPa2KRX9w%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.

No comments:

Re: [MW:35737] Bend Test and Tensile Test failed for ET45 Micro Welded Coupon

Hi As its %elongation is very low  Better try buttering on jt surrace with ductile consumable like pure Ni i. E Ni1 And later weld jt with c...