[MW:23045] Re: Diff. in ASME Sec. VIII Div-1&2

Hi,
 
Please note that the div-1 uses higher factor of safety (higher material thickness and higher material requirement) whereas div-2 uses lower factor of safety (lower thickness and lower material requirement .
 
For div-1 --> Allowable Stress = 67% of Yield Stress @ design temp
For div-2--> Allowable Stress = 90% of Yield Stress @ design temp
 
Thanks,
Kapil

On Sunday, March 6, 2011 at 9:04:08 PM UTC+5:30, prashant pansare wrote:
Dear All,
What is major difference between ASME SEC.- VIII Div- 1 & Div- 2.
Thanx & Regds,
psp

--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
Visit this group at http://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/99a7ad99-d025-4006-8cc7-b29d28e0a456%40googlegroups.com.
For more options, visit https://groups.google.com/d/optout.

No comments:

Re: [MW:35289] Welding consumable for S355J2WP material

S355 J2 WP  is a weathering structural steel  It has better atmospheric corrosion resistance. Use E 8018 - W1/W2  Electrodes This is regular...