Monday, April 6, 2015

[MW:23046] why Hardness dropped after weld repair on base metal

Hello Experts

We welded 4130 to itself ,and we performed PWHT in 1175 for 2 hours,hardness on that time was OK in base metal ,we found crack in Toe weld part we removed crack and welded with same WPS but hardness after repair dropped.

why it happened , would you please tell me what`s possibilities to made this problem?


Thanks

--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
Visit this group at http://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/b134de3f-0657-4073-8282-a65f49a03e2b%40googlegroups.com.
For more options, visit https://groups.google.com/d/optout.

No comments:

Re: [MW:35289] Welding consumable for S355J2WP material

S355 J2 WP  is a weathering structural steel  It has better atmospheric corrosion resistance. Use E 8018 - W1/W2  Electrodes This is regular...