Tuesday, February 3, 2015

Re: [MW:22796] JIS SS 41 MATERIAL

Dear Hesham,

JIS 3101 SS400 (SS 41) is equivalent to ASTM A36 in mechanical properties except elongation. You can use ER70S-X and E70XX for Welding. See the below link for further details.



Regards,
LALU
LINKS MIDDLE EAST

Thanks & Regards,

LALU R.P
+971501594161
+917566118890

On Mon, Feb 2, 2015 at 1:23 PM, 'KASHKOUSHA' via Materials & Welding <materials-welding@googlegroups.com> wrote:
Dear all
kindly, what is the equivalent of the material JIS SS 41& the suitable filler metal for welding
Thanks for your cooperation
Regards

Hesham
 
H.KASHKOUSHA

--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
Visit this group at http://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/330449626.799446.1422868999662.JavaMail.yahoo%40mail.yahoo.com.
For more options, visit https://groups.google.com/d/optout.

--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
Visit this group at http://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/CAOwU13uGwCZtAN9_PC8LNthf9xTMEV7TjxDMpy%3D3K4FEsWdLQQ%40mail.gmail.com.
For more options, visit https://groups.google.com/d/optout.

No comments:

Re: [MW:35354] Cast-iron welding

1. Preheat joint area(other area, cover with mineral wool). 2. ENiCi or ENiFe-CI. 3. stringer bead. 4. peening is to be done on weldmetal im...