Re: [MW:22795] leak in welded joint

The detection of defects by RT is limited by a certain number of factors like:

Density
Penetration
Geometrical unsharpness
 
You have to thoroughly review your RTs for Code compliance
best regards

Dr. Georgios Dilintas

Authorized Nuclear Inspector
Authorized Inspector Supervisor

I&F REGIONAL TECHNICAL MANAGER
BUREAU VERITAS PIRAEUS - GREECE

Tel: +30 210 40 63 113 /4 /5
Fax: +30 210 40 63 118
Cell: +30 69 44 64 62 04


"'raouf salhi' via Materials & Welding" ---03/02/2015 05:10:16---Dear experts; We have a skid of piping 10 " and 2 " API 5L welded and inspected according B 31.3.

From: "'raouf salhi' via Materials & Welding" <materials-welding@googlegroups.com>
To: "materials-welding@googlegroups.com" <materials-welding@googlegroups.com>
Date: 03/02/2015 05:10
Subject: [MW:22791] leak in welded joint
Sent by: materials-welding@googlegroups.com





Dear experts;

We have a skid of piping 10 " and 2 " API 5L welded and inspected according B 31.3.

we made already the internal hydro test (  two houres at 375 bar) in workshop and the result was satisfactory , we repeat the same hydrotest in the client workshop and we found a leak in one 2 " joints.

the RT report for this weld mention only undercut ( acceptable).

how we can explain this ?

regards

SALHI Raouf
QA/QC Engineer

--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to
materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to
materials-welding@googlegroups.com.
Visit this group at
http://groups.google.com/group/materials-welding.
To view this discussion on the web visit
https://groups.google.com/d/msgid/materials-welding/581386843.973075.1422885025165.JavaMail.yahoo%40mail.yahoo.com.
For more options, visit
https://groups.google.com/d/optout.

This message contains confidential information. To know more, please click on the following link: http://disclaimer.bureauveritas.com

No comments:

Re: [MW:35354] Cast-iron welding

1. Preheat joint area(other area, cover with mineral wool). 2. ENiCi or ENiFe-CI. 3. stringer bead. 4. peening is to be done on weldmetal im...