[MW:22664] Re: Comparision of UT & RT ( Justifying UT )

Pls explain in brief about Acceptance criteria comparison for RT,UT, PT (Casting/ Forging) as per ASME, EN,ASTM standards?

On Friday, July 4, 2008 12:23:26 PM UTC+5:30, vhr...@gmail.com wrote:
Dear All,
 
We awared Hydro power project. There is specifically requirments of NDT method RT for all weld joint ( i.e for all class of joint ).
 
We never used RT in normal practice for all project. Now for convince to client We required comparision sheet between RT & UT to justifying UT is better than RT.
 
Request to send Comparision of RT & UT. Please send comparision & revert back soon. We have to submitt QAP urgentely.
 
 
Regards,
 
Vikas Rana
 

--
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
To post to this group, send email to materials-welding@googlegroups.com.
Visit this group at http://groups.google.com/group/materials-welding.
To view this discussion on the web visit https://groups.google.com/d/msgid/materials-welding/2de5b950-c3ff-4b99-9dc2-b89cdde86c90%40googlegroups.com.
For more options, visit https://groups.google.com/d/optout.

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...