Wednesday, June 18, 2014

Re: [MW:21160] PWHT for stainless steel weld joint

Shot peen, laser peen, but do NOT cool slowly thru the range 850 C to 500 C  after a higher temperature treatment.

Ed Dalder


Dalder Materials Consulting, Inc.
1008 Camellia Drive
Alameda, CA 94502, U.S.A.
510-523-3649


From: "Sayee Raghunathan" <sayee1@gmail.com>
To: materials-welding@googlegroups.com
Sent: Monday, June 9, 2014 7:42:07 AM
Subject: Re: [MW:21046] PWHT for stainless steel weld joint

You need to go to basics and understand the factors influencing residual stresses which are primarily the expansion of adjoining members due to the applied heat during welding and the uneven shrinkage of the weld metal due to change of state and the weld bead shape.  Any factors which will reduce either will minimise residual stresses. In austenitic stainless steels, some methods to minimise residual stresses are use of a keyhole process such as PAW or LBW with high travel speeds and use of cryogenic gases on weld (top face or back face). 

I would also like to add that sensitisation is a time temperature dependant phenomenon, and for general low carbon grades such as 304L and 316L, upto 24hours cumulative stress relief PWHT at 610C will not cause sensitisation. For other grades similar sensitisation curves can be referred to ensure that PWHT will not be detrimental. The above does not however apply to weld overlays, where C migration and partial mixed zones complicate the issue.

Most importantly though, why do you want to reduce the residual stress in welds in austenitic stainless steels? 

finally, like someone else said, there are non-PWHT methods such as vibratory stress relief which may be used post welding.

Regards

Sayee

On Monday, 26 May 2014, Raneesh.PK <pkraneesh@gmail.com> wrote:
Dear all

As we know very well pwht is restricted for stainless steel   weld joint due to formation of chromium carbide(Senzitaion)

My question is how to reduce the weld stress of  stainless steel weld joint.

 Regards,

RANEESH.PK               


--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/d/optout.


--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/d/optout.

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...