E6010 can be used for root pass welding as it's excellent penetration characteristics which helps ensure complete fusion of the root pass. It is also good at preventing the internal undercut.
E7010-P1/E7010-G for capping and filling, as per our procedure above X-60 Gr it's recommend to use E7010-G.
Regards
Syed Farhan Rezvi
Project Engineer
Oman
On 10 November 2013 11:16, Sajeeb Yousuf <sajeeby@gmail.com> wrote:
I have a WPS for X-56--Can I follow this to make a WPS for X-65.I need to extent a pipe (APl 5L-X 65) with dia 1420mm and thickness 19.2.Which electrodes I can use.RgdsSAJEEB
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/groups/opt_out.
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/groups/opt_out.
No comments:
Post a Comment