Monday, November 11, 2013

Re: [MW:19244] WPS for X 65 Grade Steel

If your WPS qualification code is ASME Sec. IX you can use this WPS since X56 & X65 fall under P1 G2. But if you've qualified your WPS as per API 1104 you cannot use this WPS since X65 out of group "b". For W.T.,  diameter ranges and electrode please follow your approved WPS.

Regards,


On Sun, Nov 10, 2013 at 10:16 AM, Sajeeb Yousuf <sajeeby@gmail.com> wrote:
I have a WPS for X-56
Can I follow this to make a WPS for X-65.
I need to extent a pipe (APl 5L-X 65) with dia 1420mm and thickness 19.2.Which electrodes I can use.

Rgds
SAJEEB

 

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/groups/opt_out.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/groups/opt_out.

No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...