Dear Mr. Pandiyan,
There is a pneumatically operated flange facing machine which is ideal for site work. It is available for different flange sizes. On Sat, Nov 9, 2013 at 4:17 PM, N.Pandiyan <asn.pandiyan@gmail.com> wrote:
Thanks Mr. alagarsamySeriously I am looking for suggestion for any available 'hand operated tool' for flange face machining and surface preparation.The same handbook i am using.... the flanges already installed in FW system hydrant connection. We cannot remove the riser since, thrust block already poured. the flange face need to be machined and surface preparation to be made at location.Thanks to you once again
On Saturday, November 2, 2013 8:14:24 AM UTC+3, N.Pandiyan wrote:6" # 150 FF Flange, ASME B16.5 flange face got corrosion and damage, how to repair at location? any portable tools & equipment available for re-machining and serration making? the gasket type is synthetic fibre.--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/groups/opt_out.
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/groups/opt_out.
Comments