[MW:19155] Impact test for inconel material

Dear experts,

 

Please provide  mechanical test  need to qualify PQR for Inconel material as per specification.

 

Piping material Specification                                           - ASTM B444 UNS NO6625 GR.I ( CU-NI)

Pipe thickness/schedule                                                   - 80 SCH

Pipe Inch                                                                              - 1"

Design Temp                                                                      - -20/220 F
 
Please take advise us as soon as possible.
 
Note : Toughness is required or not?

 

Regards,

 

Jain,

QC Engineer

055822475



--
Regards & Thanks,

Jainul Abudeen.A
QA/QC Engineer,
Punj Lloyd Ltd.,
+918861133635


SAVE PAPER - SAVE TREE - Please do not print this e-mail unless necessary.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/groups/opt_out.

No comments:

[MW:35346] Cast-iron welding

Any advice for cast iron welding Sent from Yahoo Mail for iPhone