BK

Thanks but we do not have any design or specifications only part no as all machines supplier will never give you these details 
so what do you think the grade of steel 


On Monday, October 28, 2013 9:37 PM, BK <sarav91k@gmail.com> wrote:
Dear Hany

At this condition cannot be repaired, it has to be cut and re-welded, mouse holes should be considered at the corners to manage triaxial forces and the final fillet weld in the compound joint should be concave. Also refer to design code and calculations ...

Moreover find-out root cause for failure ...

On Monday, October 28, 2013 2:58:02 PM UTC+5:30, hany alfy wrote:

Dear Experts

Regarding the A/M Subject please find attached photos for Crane Manitowc support beams 

I Need your opinion what will be the grade of this beam and how to repair the cracks in these photos

Regards,
H.A


No comments:

[MW:35692]

Dear all    Can I do MPI above painting surface for cs  tank  Regards, Sriram Srinivasan -- https://materials-welding.blog...