Dear Ramesh

I dont think it's because of code requirement.

I believe that it would be because of smaw's disadvantage of having slag on either side of weldment once a root pass is being made, and cleaning of slag is impossible on the ID weldment if the diameter is small or inaccessible.
on the otherhand gtaw dont have slag and the client may think of gtaw's advantages over smaw's disadvantages.

Thanks
Raj

Sent from Yahoo! Mail on Android



From: Ramesh Meka <mramesh3571@gmail.com>;
To: <materials-welding@googlegroups.com>;
Subject: [MW:18325] Is SMAW is restricted to small bore pipe i.e., below 50 NB
Sent: Fri, Aug 2, 2013 4:34:28 AM

Dear Experts!
            At our project Hydraulic service pipe line is there, we
have to weld the 15 NB size, A312 TP-304L material pipe (butt & socket
joints). So, our client suggest that go for GTAW and please tell me in
which code it is given as my client said.


Thanks in advance

M.Ramesh,
Mob.+918456805540.

*Please consider the environment before printing this email.*

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm

The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/groups/opt_out.


--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/groups/opt_out.
 
 

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...