Hi, The ERNiCr-3 filler metal is well suited for such a dissimilar joint. Regards Badri --- En date de : Lun 6.5.13, shahzad <shehzadqc@gmail.com> a écrit :
De: shahzad <shehzadqc@gmail.com> Objet: [MW:17609] Welding of SS-310 to Incoloy 800 À: materials-welding@googlegroups.com Date: Lundi 6 mai 2013, 14h01
Dears Hi,
We wana weld SS-310 to Incoloy 800, could we get a sound weld by using ER-310 filler for dissimilar joint. Would it cause cracking of the dissimilar weld with ER-310 filler. Normally NiCr base fillers (F # 43) are used for these kind of dissimilar welds.
Regards. -- To post to this group, send email to materials-welding@googlegroups.com To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com For more options, visit this group's bolg at http://materials-welding.blogspot.com/http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents. --- You received this message because you are subscribed to the Google Groups "Materials & Welding" group. To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com. For more options, visit https://groups.google.com/groups/opt_out.
|
--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at
http://materials-welding.blogspot.com/ http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit
https://groups.google.com/groups/opt_out.
No comments:
Post a Comment