Monday, May 6, 2013

[MW:17607] Re: Impact test for A106 - B31.3

Assuming you are asking for Gr B (refer Fig 323.2.2A,  falls under Curve B). what is your project amb temp? if it is colder than zero you might consider that temp, else imapct test at zero deg C is required for 35mm thickness.

On Monday, May 6, 2013 3:48:37 PM UTC+5:30, anhtrang nghieng wrote:

Dear Experts,

 Process piping with material A106- thickness = 35 mm, design temp: 0 - 150 °C . My question: As per ASME B31.3, impact test for weld joint is required or not? If required, what temperature to impact test?

 

Thanks!

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
---
You received this message because you are subscribed to the Google Groups "Materials & Welding" group.
To unsubscribe from this group and stop receiving emails from it, send an email to materials-welding+unsubscribe@googlegroups.com.
For more options, visit https://groups.google.com/groups/opt_out.
 
 

No comments:

Re: [MW:35289] Welding consumable for S355J2WP material

S355 J2 WP  is a weathering structural steel  It has better atmospheric corrosion resistance. Use E 8018 - W1/W2  Electrodes This is regular...