RE: [MW:16093] Alternative welding consumable for E7018-B2L

The E-8018-B2L IS DELETED IN 1981 AND REPLACED BY E-7018-B2L, AND I FOUND IT IN THE MARKET
 

Date: Fri, 30 Nov 2012 14:06:09 +0800
From: pb.hegde@yahoo.com
Subject: Re: [MW:16084] Alternative welding consumable for E7018-B2L
To: materials-welding@googlegroups.com

You can use E8018B2L

--- On Thu, 29/11/12, sudalai kannan <sudalaims@gmail.com> wrote:

From: sudalai kannan <sudalaims@gmail.com>
Subject: [MW:16076] Alternative welding consumable for E7018-B2L
To: materials-welding@googlegroups.com
Date: Thursday, 29 November, 2012, 7:08 PM

Dear Experts,

I have repair works on 100mm thick drum, Client refered to us use E7018-B2L, but I could not found this consumable in the market. Can u guide me which electrode can use instead off E7018-B2L and what is the different between E7018-1 & E7018-B2L.


Thanks to all.


Regards,

M.Sudalai.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
 
 

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
 
 

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...