Dear Sir,

What is the specification of the material that is to be welded? Also D&H, ADOR and ESAB is having the electrode E7018-B2L. This is a commonly available brand, surprise to hear that you are not getting it.

Also please refer ASME Sec II C (Check it based on the SFA number you required) for understanding the difference. 

Regards,

Hareesh K V
+91-8306703707


On Thu, Nov 29, 2012 at 7:08 PM, sudalai kannan <sudalaims@gmail.com> wrote:

Dear Experts,

I have repair works on 100mm thick drum, Client refered to us use E7018-B2L, but I could not found this consumable in the market. Can u guide me which electrode can use instead off E7018-B2L and what is the different between E7018-1 & E7018-B2L.


Thanks to all.


Regards,

M.Sudalai.

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
 
 

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
 
 

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...