Re: [MW:16044] DIFFERENCE BETWEEN ER70S-2 &ER70S-6

ER 70S-2 is a deoxidized solid bare wire, used in GMAW of unalloyed steels.

ER70S-3 is copper coated solid bare Si Mn wire, used for GTAW of unalloyed steels applications.

Both of them can be used for general construction works like vessels, ship building etc.

The last digit signifies the chemical composition of the weld metal (Suffix 'GS' is intended for single pass welds only).

ವಂದನೆಗಳೊಂದಿಗೆ / Best regards,

Nandesh Kumar A

Abu Dhabi, UAE

P.S. : Please don't print this e-mail unless you really need to.


--- On Mon, 26/11/12, Vinu Raveendran <vinuravi007@gmail.com> wrote:

From: Vinu Raveendran <vinuravi007@gmail.com>
Subject: [MW:16039] DIFFERENCE BETWEEN ER70S-2 &ER70S-6
To: materials-welding@googlegroups.com
Date: Monday, 26 November, 2012, 8:19 AM

Dear Members,

I would like to know difference between ER70S2 &ER70S6?
What does "2" and "6" mean in them and which welding process we use them?

Thankyou! 

--
VINU RAVEENDRAN

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
 
 

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
 
 

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...