Sunday, November 25, 2012

Re: [MW:16035] Maximum Operating Temp. for UT

In case of thickness measurment by using UT can be measured for High-temperature materials, up to about 540°C (1000°F), with specially designed instruments with high-temperature compensation, search unit assemblies, and couplants. Refer SE-797 of ASME Sec V.
 
Regards
Sudhir Kumar

On Sat, Nov 24, 2012 at 6:40 AM, Vicky Patil <patilvicky4@gmail.com> wrote:
Dear Experts,

What is the maximum allowable temperature to carry out UT?

Regards,

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
 
 

--
To post to this group, send email to materials-welding@googlegroups.com
To unsubscribe from this group, send email to materials-welding+unsubscribe@googlegroups.com
For more options, visit this group's bolg at http://materials-welding.blogspot.com/
http://www.linkedin.com/groups/MaterialsWelding-122787?home=&gid=122787&trk=anet_ug_hm
 
The views expressed/exchnaged in this group are members personel views and meant for educational purposes only, Users must take their own decisions w.r.t. applicable code/standard/contract documents.
 
 

No comments:

Re: [MW:35686] HDPE WPS

Refer ASME SEC IX  There is separate chapter for Plastic welding . Based on that you have to prepare  Sent from my iPhone On 21 Jun 2025, at...